Keyword
16 micrographs for keyword coring, ordered by micrograph number.
| Showing 1 - 10 of 16 micrographs | Page 1 2 | Previous | Next |
![]() |
Micrograph
10
:
Cu 70, Ni 30 (wt%), cored dendrites System: Cu-Ni, Composition: Cu 70, Ni 30 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
11
:
Cu 70, Ni 30 (wt%), cored dendrites System: Cu-Ni, Composition: Cu 70, Ni 30 (wt%) Reflected light microscopy 80 μm |
![]() |
Micrograph
47
:
Al 95, Cu 5 (wt%), microsegregation - cored dendrites System: Al-Cu, Composition: Al 95, Cu 5 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
48
:
Al 95, Cu 5 (wt%), microsegregation - cored dendrites System: Al-Cu, Composition: Al 95, Cu 5 (wt%) Reflected light microscopy 80 μm |
![]() |
Micrograph
516
:
Gun metal bronze displaying coring. System: Cu-Sn, Composition: Cu 88, Sn 8, Zn 4 (wt% approx) Reflected light microscopy 800 μm |
![]() |
Micrograph
517
:
Gun metal bronze displaying coring. System: Cu-Sn, Composition: Cu 88, Sn 8, Zn 4 (wt% approx) Reflected light microscopy 400 μm |
![]() |
Micrograph
518
:
Gun metal bronze displaying coring. System: Cu-Sn, Composition: Cu 88, Sn 8, Zn 4 (wt% approx) Reflected light microscopy 200 μm |
![]() |
Micrograph
519
:
Gun metal bronze displaying coring. System: Cu-Sn, Composition: Cu 88, Sn 8, Zn 4 (wt% approx) Reflected light microscopy 100 μm |
![]() |
Micrograph
523
:
Phosphor bronze exhibiting cored dendrites. System: Cu-Sn, Composition: Cu 90, Sn 10 (wt%) + P trace Reflected light microscopy 400 μm |
![]() |
Micrograph
524
:
Phosphor bronze exhibiting cored dendrites. System: Cu-Sn, Composition: Cu 90, Sn 10 (wt%) + P trace Reflected light microscopy 200 μm |