Keyword
58 micrographs for keyword composite material, ordered by micrograph number.
| Showing 51 - 58 of 58 micrographs | Page 1 2 3 4 5 6 | Previous | Next |
![]() |
Micrograph
634
:
Solid-gas eutectic solidification (Gasar) aluminium foam System: Al, Composition: Not specified Photography (no microscope) 120 μm |
![]() |
Micrograph
635
:
Open celled aluminium foam produced by infiltration of sintered salt System: Al, Composition: Not specified Scanning electron microscopy (SEM) 400 μm |
![]() |
Micrograph
636
:
Alporas' closed cell aluminium foam System: Al, Composition: Not specified Photography (no microscope) 6 mm |
![]() |
Micrograph
670
:
Carbon-carbon composite System: CCcomposite, Composition: Not specified Reflected light microscopy 400 μm |
![]() |
Micrograph
671
:
Carbon-carbon composite System: CCcomposite, Composition: Not specified Reflected light microscopy 200 μm |
![]() |
Micrograph
672
:
Carbon-carbon composite System: CCcomposite, Composition: Not specified Reflected light microscopy 100 μm |
![]() |
Micrograph
673
:
Carbon-carbon composite System: CCcomposite, Composition: Not specified Reflected light microscopy 50 μm |
![]() |
Micrograph
674
:
Carbon-carbon composite System: CCcomposite, Composition: Not specified Reflected light microscopy 20 μm |
| Showing 51 - 58 of 58 micrographs | Page 1 2 3 4 5 6 | Previous | Next |