Keyword
17 micrographs for keyword lamella, ordered by micrograph number.
| Showing 11 - 17 of 17 micrographs | Page 1 2 | Previous | Next |
![]() |
Micrograph
646
:
Spherulite growth imaged by atomic force microscopy (AFM) System: Polyhydroxybutyrate (PHB), Composition: Not specified Atomic force microscopy (AFM) 500 nm |
![]() |
Micrograph
665
:
Al-90 wt% Cu (bronze) System: Al-Cu, Composition: Al 10, Cu 90 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
666
:
Al-90 wt% Cu (bronze) System: Al-Cu, Composition: Al 10, Cu 90 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
667
:
Al-90 wt% Cu (bronze) System: Al-Cu, Composition: Al 10, Cu 90 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
668
:
Al-90 wt% Cu (bronze) System: Al-Cu, Composition: Al 10, Cu 90 (wt%) Reflected light microscopy 50 μm |
![]() |
Micrograph
669
:
Al-90 wt% Cu (bronze) System: Al-Cu, Composition: Al 10, Cu 90 (wt%) Reflected light microscopy 20 μm |
![]() |
Micrograph
778
:
Grey cast iron (flake graphite) System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5 (wt%) Reflected light microscopy 40 μm |
| Showing 11 - 17 of 17 micrographs | Page 1 2 | Previous | Next |