Keyword
44 micrographs for keyword austenite, ordered by micrograph number.
| Showing 11 - 20 of 44 micrographs | Page 1 2 3 4 5 | Previous | Next |
![]() |
Micrograph
772
:
Austenitic stainless steel System: Fe-C-X, Composition: Stainless steel Transmission electron microscopy (TEM) 1 μm |
![]() |
Micrograph
773
:
Austenitic stainless steel System: Fe-C-X, Composition: Stainless steel Transmission electron microscopy (TEM) 1 μm |
![]() |
Micrograph
774
:
Austenitic stainless steel System: Fe-C-X, Composition: Stainless steel Transmission electron microscopy (TEM) 1 μm |
![]() |
Micrograph
775
:
Austenitic stainless steel System: Fe-C-X, Composition: Stainless steel Transmission electron microscopy (TEM) 1 μm |
![]() |
Micrograph
776
:
Austenitic stainless steel System: Fe-C-X, Composition: Stainless steel Transmission electron microscopy (TEM) 2 μm |
![]() |
Micrograph
797
:
Wear-resistant high-chromium cast iron System: Fe-C-X, Composition: Fe, C 2.6, Cr 17, Mo 2, Ni 2 (wt%) Reflected light microscopy 40 μm |
![]() |
Micrograph
798
:
Wear-resistant high-chromium cast iron System: Fe-C-X, Composition: Fe, C 2.6, Cr 17, Mo 2, Ni 2 (wt%) Reflected light microscopy 20 μm |
![]() |
Micrograph
799
:
Austenitic stainless steel solution treated, water quenched and tempered System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%) Scanning electron microscopy (SEM) 2 μm |
![]() |
Micrograph
800
:
Austenitic stainless steel tempered System: Fe-C-X, Composition: Stainless steel with Nb 1 (wt%) Scanning electron microscopy (SEM) 1 μm |
![]() |
Micrograph
801
:
Austenitic stainless steel solution treated, water quenched then tempered System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%) Transmission electron microscopy (TEM) 400 nm |