4 micrographs for keyword allotriomorph, ordered by micrograph number.


Link to full record for micrograph 17 Micrograph 17 : Fe, C 0.1 (wt%), hypoeutectoid alloy
System: Fe-C-X, Composition: Fe, C 0.1 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 18 Micrograph 18 : Fe, C 0.1 (wt%), hypoeutectoid alloy
System: Fe-C-X, Composition: Fe, C 0.1 (wt%)
Reflected light microscopy
40 μm
Link to full record for micrograph 25 Micrograph 25 : Fe, C 0.85 (wt%), hypereutectoid alloy
System: Fe-C-X, Composition: Fe, C 0.85 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 26 Micrograph 26 : Fe, C 0.85 (wt%), hypereutectoid alloy
System: Fe-C-X, Composition: Fe, C 0.85 (wt%)
Reflected light microscopy
40 μm