Keyword
67 micrographs for keyword quenching, ordered by micrograph number.
| Showing 51 - 60 of 67 micrographs | Page 1 2 3 4 5 6 7 | Previous | Next |
![]() |
Micrograph
344
:
Medium carbon, low alloy steel. System: Fe-C-X, Composition: Fe, C 0.31, Ni 3.0, Cr 0.9, Mn 0.6 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
345
:
Medium carbon, low alloy steel, isothermally transformed System: Fe-C-X, Composition: Fe, C 0.4, Ni 1.3, Cr 0.65, Mo 0.65 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
346
:
Fe, C 1.35 (wt%) steel, hypereutectoid, quenched System: Fe-C-X, Composition: Fe, C 1.35 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
347
:
Fe, C 1.35 (wt%) steel, hypereutectoid, quenched System: Fe-C-X, Composition: Fe, C 1.35 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
348
:
Fe, C 1.35 (wt%) steel, hypereutectoid, quenched System: Fe-C-X, Composition: Fe, C 1.35 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
349
:
Fe, C 1.35 (wt%) steel, hypereutectoid, quenched System: Fe-C-X, Composition: Fe, C 1.35 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
350
:
Fe, C 0.15 (wt%) steel, quenched. System: Fe-C-X, Composition: Fe, C 0.15 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
351
:
Fe, C 0.15 (wt%) steel, quenched. System: Fe-C-X, Composition: Fe, C 0.15 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
352
:
Fe, C 0.15 (wt%) steel, quenched. System: Fe-C-X, Composition: Fe, C 0.15 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
555
:
Banded spherulites in a blend of polyethtylenes System: Polyethylene (PE), Composition: LPE:BPE 1:3 Transmission electron microscopy (TEM) 200 nm |