78 micrographs for keyword dendrite, ordered by micrograph number.
| Showing 51 - 60 of 78 micrographs | Page 1 2 3 4 5 6 7 8 | Previous | Next |
![]() |
Micrograph
509
:
D4 Leaded bronze, cored dendrites. System: Cu-Sn, Composition: Cu 85, Sn 10, Pb 5 (wt% approx) Reflected light microscopy 400 μm |
![]() |
Micrograph
510
:
D4 Leaded bronze, cored dendrites. System: Cu-Sn, Composition: Cu 85, Sn 10, Pb 5 (wt% approx) Reflected light microscopy 200 μm |
![]() |
Micrograph
511
:
D4 Leaded bronze, cored dendrites. System: Cu-Sn, Composition: Cu 85, Sn 10, Pb 5 (wt% approx) Reflected light microscopy 100 μm |
![]() |
Micrograph
523
:
Phosphor bronze exhibiting cored dendrites. System: Cu-Sn, Composition: Cu 90, Sn 10 (wt%) + P trace Reflected light microscopy 400 μm |
![]() |
Micrograph
524
:
Phosphor bronze exhibiting cored dendrites. System: Cu-Sn, Composition: Cu 90, Sn 10 (wt%) + P trace Reflected light microscopy 200 μm |
![]() |
Micrograph
525
:
Phosphor bronze exhibiting cored dendrites. System: Cu-Sn, Composition: Cu 90, Sn 10 (wt%) + P trace Reflected light microscopy 100 μm |
![]() |
Micrograph
605
:
Fracture surface formed by hot tearing (solidification cracking) System: Al, Composition: Commercial purity (99.5%) Scanning electron microscopy (SEM) 40 μm |
![]() |
Micrograph
613
:
Facetted aluminium dendrites System: Al-Sn, Composition: Al 15, Sn 85 (wt%) Reflected light microscopy 80 μm |
![]() |
Micrograph
617
:
Deeply etched Co-dendrites System: Co-Sm-Cu, Composition: Co 70, Sm 10, Cu 20 (at%) Scanning electron microscopy (SEM) 80 μm |
![]() |
Micrograph
695
:
Cu-4.5 wt% P System: Cu-P, Composition: Cu 95.5, P 4.5 (wt%) Reflected light microscopy 400 μm |
| Showing 51 - 60 of 78 micrographs | Page 1 2 3 4 5 6 7 8 | Previous | Next |