12 micrographs for keyword glass, ordered by micrograph number.
Showing 11 - 12 of 12 micrographs | Page 1 2 | Previous | Next |
![]() |
Micrograph
544
:
Devitrified Glass: glass sample heated at 900°C for 17 hours System: SiO2, Composition: Mostly silica, SiO2 Transmitted polarised light microscopy, with sensitive tint plate 250 μm |
![]() |
Micrograph
596
:
Glass-fibre reinforced polymer System: Polypropylene (PP), Composition: Polypropylene with 15% glass fibres Reflected light microscopy 400 μm |