Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Keyword
24 micrographs for keyword ductile, ordered by micrograph number.
| Showing 21 - 24 of 24 micrographs | Page 1 2 3 | Previous | Next |
![]() |
Micrograph
793
:
Austempered ductile cast iron System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
794
:
Austempered ductile cast iron System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%) Reflected light microscopy 20 μm |
![]() |
Micrograph
795
:
Blackheart cast iron System: Fe-C-X, Composition: Blackheart cast iron Reflected light microscopy 100 μm |
![]() |
Micrograph
796
:
Blackheart cast iron System: Fe-C-X, Composition: Blackheart cast iron Reflected light microscopy 100 μm |
| Showing 21 - 24 of 24 micrographs | Page 1 2 3 | Previous | Next |