1 micrograph for keyword periclase, ordered by micrograph number.
![]() |
Micrograph
192
:
Doloma, (Ca,Mg)O System: (Ca,Mg)O, Composition: CaO 57, MgO 41 (wt%), + Fe2O3, SiO2 and Al2O3 (typical) Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode 30 μm |