Keyword
2 micrographs for keyword tough ceramic, ordered by micrograph number.
![]() |
Micrograph
196
:
Tetragonal Zirconia Polycrystals (TZP) System: ZrO2-Y2O3, Composition: Y2O3 2-3, ZrO2 96-97 (wt%) Bright-field TEM 600 nm |
![]() |
Micrograph
197
:
Partially Stabilised Zirconia (PSZ) System: ZrO2-MgO, Composition: MgO 2.5-3.6, ZrO2 97.5-96.4 (wt%) Bright-field TEM 300 nm |