Keyword
23 micrographs for keyword hypoeutectoid, ordered by micrograph number.
| Showing 1 - 10 of 23 micrographs | Page 1 2 3 | Previous | Next |
![]() |
Micrograph
17
:
Fe, C 0.1 (wt%), hypoeutectoid alloy System: Fe-C-X, Composition: Fe, C 0.1 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
18
:
Fe, C 0.1 (wt%), hypoeutectoid alloy System: Fe-C-X, Composition: Fe, C 0.1 (wt%) Reflected light microscopy 40 μm |
![]() |
Micrograph
19
:
Fe, C 0.1 (wt%), hypoeutectoid alloy System: Fe-C-X, Composition: Fe, C 0.1 (wt%) Scanning electron microscopy (SEM) 30 μm |
![]() |
Micrograph
20
:
Fe, C 0.1 (wt%), hypoeutectoid alloy System: Fe-C-X, Composition: Fe, C 0.1 (wt%) Scanning electron microscopy (SEM) 10 μm |
![]() |
Micrograph
225
:
Normalised steel System: Fe-C-X, Composition: Fe, C 0.55 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
226
:
Normalised steel System: Fe-C-X, Composition: Fe, C 0.55 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
227
:
Normalised steel System: Fe-C-X, Composition: Fe, C 0.4 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
228
:
Normalised steel System: Fe-C-X, Composition: Fe, C 0.4 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
229
:
Normalised steel System: Fe-C-X, Composition: Fe, C 0.5 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
230
:
Normalised steel System: Fe-C-X, Composition: Fe, C 0.5 (wt%) Reflected light microscopy 200 μm |
| Showing 1 - 10 of 23 micrographs | Page 1 2 3 | Previous | Next |