Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Keyword
26 micrographs for keyword manganese, ordered by micrograph number.
| Showing 11 - 20 of 26 micrographs | Page 1 2 3 | Previous | Next |
![]() |
Micrograph
403
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 400 μm |
![]() |
Micrograph
404
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 200 μm |
![]() |
Micrograph
405
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 100 μm |
![]() |
Micrograph
782
:
Austempered ductile cast iron System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
783
:
Austempered ductile cast iron System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
784
:
Austempered ductile cast iron System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
785
:
Austempered ductile cast iron System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%) Reflected light microscopy 20 μm |
![]() |
Micrograph
786
:
Austempered ductile cast iron System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
787
:
Austempered ductile cast iron System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%) Reflected light microscopy 20 μm |
![]() |
Micrograph
788
:
Austempered ductile cast iron System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%) Reflected light microscopy 100 μm |
| Showing 11 - 20 of 26 micrographs | Page 1 2 3 | Previous | Next |