Keyword
18 micrographs for keyword tempered, ordered by micrograph number.
| Showing 1 - 10 of 18 micrographs | Page 1 2 | Previous | Next |
![]() |
Micrograph
294
:
Fe, C 0.75 (wt%) steel, quenched and tempered System: Fe-C-X, Composition: Fe, C 0.75 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
295
:
Fe, C 0.75 (wt%) steel, quenched and tempered System: Fe-C-X, Composition: Fe, C 0.75 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
296
:
Fe, C 0.75 (wt%) steel, quenched and tempered System: Fe-C-X, Composition: Fe, C 0.75 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
301
:
Fe, C 0.55 (wt%) steel, quenched and tempered System: Fe-C-X, Composition: Fe, C 0.55 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
302
:
Fe, C 0.55 (wt%) steel, quenched and tempered System: Fe-C-X, Composition: Fe, C 0.55 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
303
:
Fe, C 0.3 (wt%) steel, quenched and tempered System: Fe-C-X, Composition: Fe, C 0.3 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
304
:
Fe, C 0.3 (wt%) steel, quenched and tempered System: Fe-C-X, Composition: Fe, C 0.3 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
305
:
Fe, C 0.3 (wt%) steel, quenched and tempered System: Fe-C-X, Composition: Fe, C 0.3 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
313
:
Fe, C 0.9 (wt%) steel, hypereutectoid, quenched and tempered System: Fe-C-X, Composition: Fe, C 0.9 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
314
:
Fe, C 0.9 (wt%) steel, hypereutectoid, quenched and tempered System: Fe-C-X, Composition: Fe, C 0.9 (wt%) Reflected light microscopy 200 μm |