Micrograph
628
:
Sintered salt (NaCl) System: Na-Cl, Composition: Not specified Scanning electron microscopy (SEM) 140 μm |
![]() |
Micrograph
650
:
Small ceramic pot showing centimetre scale crystals within the glaze System: Soda-lime-silica glaze, Composition: Soda-lime-silica glaze containing zinc oxide 25, cobalt oxide 0.5 (wt%) Photography (no microscope) 20 mm |
![]() |
Micrograph
655
:
Small ceramic pot showing centimetre scale crystals within the glaze System: Soda-lime-silica glaze, Composition: Soda-lime-silica glaze containing zinc oxide 25, cobalt oxide 0.5 (wt%) Photography (no microscope) 5 mm |
![]() |
Micrograph
663
:
Barium titanate ceramic System: BaTiO3, Composition: Not specified Reflected light microscopy No length bar |
![]() |
Micrograph
664
:
Barium titanate ceramic System: BaTiO3, Composition: Not specified Reflected light microscopy No length bar |
![]() |
Micrograph
675
:
Magnesia-Chromite Clinker System: Magnesia chromite, Composition: Magnesia 85, chromite 15 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
676
:
Magnesia-Chromite Clinker System: Magnesia chromite, Composition: Magnesia 85, chromite 15 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
677
:
Magnesia-Chromite Clinker System: Magnesia chromite, Composition: Magnesia 85, chromite 15 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
678
:
Magnesia-Chromite Clinker System: Magnesia chromite, Composition: Magnesia 85, chromite 15 (wt%) Reflected light microscopy 50 μm |
![]() |
Micrograph
679
:
BaO-Nd2O3-4TiO2 System: BaO-Nd2O3-4TiO2, Composition: Not specified Reflected light microscopy 400 μm |