Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Keyword
2 micrographs for keyword craze remnants, ordered by micrograph number.
![]() |
Micrograph
589
:
Remnants of crazes on a polystyrene fracture surface System: Polystyrene (PS), Composition: Not specified Scanning electron microscopy (SEM) 8 μm |
![]() |
Micrograph
590
:
Remnants of crazes on a polycarbonate fracture surface System: Polycarbonate (PC), Composition: Not specified Scanning electron microscopy (SEM) 10 μm |