16 micrographs for keyword grey cast iron, ordered by micrograph number.
| Showing 11 - 16 of 16 micrographs | Page 1 2 | Previous | Next |
![]() |
Micrograph
389
:
Silal System: Fe-C-X, Composition: Fe, C 2.10, Si 5.60, Mn 0.50 (wt%) (Silal) Reflected light microscopy 100 μm |
![]() |
Micrograph
777
:
Grey cast iron (flake graphite) System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
778
:
Grey cast iron (flake graphite) System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5 (wt%) Reflected light microscopy 40 μm |
![]() |
Micrograph
779
:
Spheroidal graphite cast iron System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5, Mg 0.05 (wt%) Reflected light microscopy 50 μm |
![]() |
Micrograph
780
:
Heat treated spheroidal graphite cast iron System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5, Mg 0.05 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
781
:
Heat treated spheroidal graphite cast iron System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5, Mg 0.05 (wt%) Reflected light microscopy 50 μm |