Keyword
3 micrographs for keyword elongation, ordered by micrograph number.
![]() |
Micrograph
604
:
Extruded aluminium System: Al, Composition: Commercial purity (99.5%) Reflected light microscopy, polarised 40 μm |
![]() |
Micrograph
608
:
Channelling contrast TEM image of subgrains of extruded aluminium System: Al, Composition: Commercial purity (99.5%) Transmission electron microscopy (TEM) 600 nm |
![]() |
Micrograph
609
:
The grain structure of extruded aluminium System: Al, Composition: Commercial purity (99.5%) Reflected light microscopy, polarised 40 μm |