12 micrographs for keyword extrusion, ordered by micrograph number.
Showing 11 - 12 of 12 micrographs | Page 1 2 | Previous | Next |
![]() |
Micrograph
725
:
Ni-Superalloy, as-extruded microstructure System: Ni-X, Composition: Ni, Cr 14.4-15.2, Co 13-18, Mo 3.5-4.5, Al 3.0-3.3, Ti 4.2-4.8, Ta 2.5, Zr 0.05-0.07, C 0.05, B 0.01-0.03 (wt%) (Ni-Superalloy) Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode 10 μm |
![]() |
Micrograph
734
:
Ni-Superalloy, as-extruded microstructure System: Ni-X, Composition: Ni, Cr 14.4-15.2, Co 13-18, Mo 3.5-4.5, Al 3.0-3.3, Ti 4.2-4.8, Ta 2.5, Zr 0.05-0.07, C 0.05, B 0.01-0.03 (wt%) (Ni-Superalloy) Transmission electron microscopy (TEM) of carbon replica 20 μm |