18 micrographs for keyword hypereutectoid, ordered by micrograph number.
| Showing 11 - 18 of 18 micrographs | Page 1 2 | Previous | Next |
![]() |
Micrograph
247
:
Fe, C 1.3 (wt%) steel, normalised at 1050°C System: Fe-C-X, Composition: Fe, C 1.3 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
248
:
Fe, C 1.3 (wt%) steel, annealed at 1000°C System: Fe-C-X, Composition: Fe, C 1.3 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
249
:
Fe, C 1.3 (wt%) steel, annealed at 1000°C System: Fe-C-X, Composition: Fe, C 1.3 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
250
:
Fe, C 1.3 (wt%) steel, annealed at 1000°C System: Fe-C-X, Composition: Fe, C 1.3 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
253
:
Fe, C 1 (wt%) steel, normalised hypereutectoid System: Fe-C-X, Composition: Fe, C 1.0 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
254
:
Fe, C 1 (wt%) steel, normalised hypereutectoid System: Fe-C-X, Composition: Fe, C 1.0 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
255
:
Fe, C 1.1 (wt%) steel, normalised hypereutectoid System: Fe-C-X, Composition: Fe, C 1.1 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
256
:
Fe, C 1.1 (wt%) steel, normalised hypereutectoid System: Fe-C-X, Composition: Fe, C 1.1 (wt%) Reflected light microscopy 200 μm |