Keyword
1 micrograph for keyword glass fibre reinforced composite, ordered by micrograph number.
![]() |
Micrograph
596
:
Glass-fibre reinforced polymer System: Polypropylene (PP), Composition: Polypropylene with 15% glass fibres Reflected light microscopy 400 μm |