3 micrographs for keyword intergranular, ordered by micrograph number.
![]() |
Micrograph
78
:
Forging steel, brittle, intergranular fracture System: Fe-C-X, Composition: Forging steel Scanning electron microscopy (SEM) 800 μm |
![]() |
Micrograph
146
:
HY100 forging steel, notched impact specimen, failed through brittle intergranular fracture. System: Fe-C-X, Composition: Not specified Scanning electron microscopy (SEM) 200 μm |
![]() |
Micrograph
147
:
HY100 forging steel, notched impact specimen, failed through brittle intergranular fracture. System: Fe-C-X, Composition: Not specified Scanning electron microscopy (SEM) 200 μm |