5 micrographs for keyword infiltration, ordered by micrograph number.
![]() |
Micrograph
602
:
Section of a metal matrix composite (MMC) System: Al-Mg, Composition: Al, Mg 2.5 (wt%), with Al2O3 (10 vol%) Reflected light microscopy, polarised 80 μm |
![]() |
Micrograph
603
:
Section of a metal matrix composite (MMC) System: Al-Mg, Composition: Al, Mg 2.5 (wt%), with Al2O3 (5 vol%) Reflected light microscopy, polarised 80 μm |
![]() |
Micrograph
607
:
Fibre fracture in a metal matrix composite System: Al, Composition: Commercial purity (99.5%) Scanning electron microscopy (SEM) 4 μm |
![]() |
Micrograph
631
:
Coarse open celled aluminium foam produced by infiltration of sintered salt (FOAM-U-LIKE) System: Al, Composition: Not specified Photography (no microscope) 6 mm |
![]() |
Micrograph
635
:
Open celled aluminium foam produced by infiltration of sintered salt System: Al, Composition: Not specified Scanning electron microscopy (SEM) 400 μm |