71 micrographs for keyword martensite, ordered by micrograph number.
| Showing 31 - 40 of 71 micrographs | Page 1 2 3 4 5 6 7 8 | Previous | Next |
![]() |
Micrograph
318
:
Fe, C 0.9 (wt%) steel, hypereutectoid, quenched System: Fe-C-X, Composition: Fe, C 0.9 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
326
:
Low alloy medium carbon steel, isothermally transformed System: Fe-C-X, Composition: Fe, C 0.4, Ni 1.3, Cr 0.65, Mo 0.65 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
327
:
Low alloy medium carbon steel, isothermally transformed System: Fe-C-X, Composition: Fe, C 0.4, Ni 1.3, Cr 0.65, Mo 0.65 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
328
:
Nickel low carbon steel, quenched and tempered System: Fe-C-X, Composition: Fe, C 0.31, Ni 3.0, Cr 0.9, Mn 0.6 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
329
:
Nickel low carbon steel, quenched and tempered System: Fe-C-X, Composition: Fe, C 0.31, Ni 3.0, Cr 0.9, Mn 0.6 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
330
:
Near eutectoid steel, quenched to produce martensite System: Fe-C-X, Composition: Fe, C 0.86 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
331
:
Near eutectoid steel, quenched to produce martensite System: Fe-C-X, Composition: Fe, C 0.86 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
332
:
Fe, C 0.86 (wt%) steel, quenched, cracked System: Fe-C-X, Composition: Fe, C 0.86 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
336
:
Medium carbon steel, quenched System: Fe-C-X, Composition: Fe, C 0.3 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
337
:
Fe, C 1.35 (wt%) steel, quenched System: Fe-C-X, Composition: Fe, C 1.35 (wt%) Reflected light microscopy 200 μm |