Keyword

535 micrographs for keyword alloy, ordered by micrograph number.


Showing 171 - 180 of 535 micrographs Page 1 .. 15 16 17 18 19 20 21 .. 54 | Previous | Next

Link to full record for micrograph 275 Micrograph 275 : Fe, C 0.07, Mn 2.3 (wt%) steel, carburised at 950°C
System: Fe-C-X, Composition: Fe, C 0.07, Mn 2.2 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 276 Micrograph 276 : Fe, C 0.07, Mn 2.3 (wt%) steel, carburised at 950°C
System: Fe-C-X, Composition: Fe, C 0.07, Mn 2.2 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 277 Micrograph 277 : Fe, C 0.07, Mn 2.3 (wt%) steel, carburised at 950°C
System: Fe-C-X, Composition: Fe, C 0.07, Mn 2.2 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 278 Micrograph 278 : Fe, C 2, Mn 0.7 (wt%) steel, quenched, producing martensite
System: Fe-C-X, Composition: Fe, C 0.55, Mn 0.65 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 279 Micrograph 279 : Fe, C 2, Mn 0.7 (wt%) steel, quenched, producing martensite and cracking
System: Fe-C-X, Composition: Fe, C 0.55, Mn 0.65 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 280 Micrograph 280 : Fe, C 2, Mn 0.7 (wt%) steel, quenched, producing martensite and cracking
System: Fe-C-X, Composition: Fe, C 0.55, Mn 0.65 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 281 Micrograph 281 : Fe, C 0.2 (wt%) steel, case hardened
System: Fe-C-X, Composition: Fe, C 0.2 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 282 Micrograph 282 : Fe, C 0.2 (wt%) steel, case hardened
System: Fe-C-X, Composition: Fe, C 0.2 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 283 Micrograph 283 : Fe, C 0.2 (wt%) steel, case hardened
System: Fe-C-X, Composition: Fe, C 0.2 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 284 Micrograph 284 : Fe, C 0.2 (wt%) steel, case hardened
System: Fe-C-X, Composition: Fe, C 0.2 (wt%)
Reflected light microscopy
100 μm

Showing 171 - 180 of 535 micrographs Page 1 .. 15 16 17 18 19 20 21 .. 54 | Previous | Next