535 micrographs for keyword alloy, ordered by micrograph number.
| Showing 351 - 360 of 535 micrographs | Page 1 .. 33 34 35 36 37 38 39 .. 54 | Previous | Next |
![]() |
Micrograph
469
:
Cu 50, Zn 50 (wt%) brass, as cast System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
470
:
Cu 50, Zn 50 (wt%) brass, as cast System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
471
:
Cu 50, Zn 50 (wt%) brass, as cast System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
472
:
Cu 50, Zn 50 (wt%) brass, chill cast System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
473
:
Cu 50, Zn 50 (wt%) brass, chill cast System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
474
:
Cu 50, Zn 50 (wt%) brass, chill cast System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
475
:
Cu 55, Zn 45 (wt%) brass, cast annealed System: Cu-Zn, Composition: Cu 52, Zn 45 (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
476
:
Cu 55, Zn 45 (wt%) brass, cast annealed System: Cu-Zn, Composition: Cu 52, Zn 45 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
477
:
Cu 80, Zn 20 (wt%) brass, exhibiting dendritic solidification System: Cu-Zn, Composition: Cu 80, Zn 20 (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
478
:
Cu 80, Zn 20 (wt%) brass, exhibiting dendritic solidification System: Cu-Zn, Composition: Cu 80, Zn 20 (wt%) Reflected light microscopy 200 μm |
| Showing 351 - 360 of 535 micrographs | Page 1 .. 33 34 35 36 37 38 39 .. 54 | Previous | Next |