Keyword
535 micrographs for keyword alloy, ordered by micrograph number.
| Showing 441 - 450 of 535 micrographs | Page 1 .. 42 43 44 45 46 47 48 .. 54 | Previous | Next |
![]() |
Micrograph
660
:
Al-4 wt% Cu, over aged alloy System: Al-Cu, Composition: Al 96, Cu 4 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
661
:
Al-4 wt% Cu, over aged alloy System: Al-Cu, Composition: Al 96, Cu 4 (wt%) Reflected light microscopy 50 μm |
![]() |
Micrograph
662
:
Al-4 wt% Cu, over aged alloy System: Al-Cu, Composition: Al 96, Cu 4 (wt%) Reflected light microscopy 20 μm |
![]() |
Micrograph
665
:
Al-90 wt% Cu (bronze) System: Al-Cu, Composition: Al 10, Cu 90 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
666
:
Al-90 wt% Cu (bronze) System: Al-Cu, Composition: Al 10, Cu 90 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
667
:
Al-90 wt% Cu (bronze) System: Al-Cu, Composition: Al 10, Cu 90 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
668
:
Al-90 wt% Cu (bronze) System: Al-Cu, Composition: Al 10, Cu 90 (wt%) Reflected light microscopy 50 μm |
![]() |
Micrograph
669
:
Al-90 wt% Cu (bronze) System: Al-Cu, Composition: Al 10, Cu 90 (wt%) Reflected light microscopy 20 μm |
![]() |
Micrograph
695
:
Cu-4.5 wt% P System: Cu-P, Composition: Cu 95.5, P 4.5 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
696
:
Cu-4.5 wt% P System: Cu-P, Composition: Cu 95.5, P 4.5 (wt%) Reflected light microscopy 200 μm |
| Showing 441 - 450 of 535 micrographs | Page 1 .. 42 43 44 45 46 47 48 .. 54 | Previous | Next |