535 micrographs for keyword alloy, ordered by micrograph number.


Showing 461 - 470 of 535 micrographs Page 1 .. 44 45 46 47 48 49 50 .. 54 | Previous | Next

Link to full record for micrograph 707 Micrograph 707 : Cu-? wt% P
System: Cu-P, Composition: Not specified
Reflected light microscopy
100 μm
Link to full record for micrograph 708 Micrograph 708 : Cu-? wt% P
System: Cu-P, Composition: Not specified
Reflected light microscopy
50 μm
Link to full record for micrograph 709 Micrograph 709 : Cu-? wt% P
System: Cu-P, Composition: Not specified
Reflected light microscopy
20 μm
Link to full record for micrograph 710 Micrograph 710 : Wrought-grade aluminium alloy (Al-Mg-Fe-Si containing < 1wt.% of each solute); refined with TiB2 particles. Deformation of grain structure is due to cutting of sample with scissors.
System: Al-Mg-Fe-Si, Composition: Not specified
Cross-polarised light microscopy
400 μm
Link to full record for micrograph 711 Micrograph 711 : As-cast wrought-grade aluminium alloy (Al-Mg-Fe-Si containing < 1wt.% of each solute). No addition of grain refinement particles (e.g. TiB2).
System: Al-Mg-Fe-Si, Composition: Not specified
Cross-polarised light microscopy
1 mm
Link to full record for micrograph 712 Micrograph 712 : As-cast wrought-grade aluminium alloy (Al-Mg-Fe-Si containing < 1wt.% of each solute). Addition of TiB2 particles facilitates the formation of a fine, equiaxed grain structure (grain refinement).
System: Al-Mg-Fe-Si, Composition: Not specified
Cross-polarised light microscopy
400 μm
Link to full record for micrograph 713 Micrograph 713 : IN718 nickel-based superalloy held for 1 minute at 850°C
System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al
Reflected light microscopy, cross-polarised, with Nomarski filter
20 μm
Link to full record for micrograph 714 Micrograph 714 : IN718 nickel-based superalloy held for 20 minutes at 850°C
System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al
Reflected light microscopy, cross-polarised, with Nomarski filter
20 μm
Link to full record for micrograph 715 Micrograph 715 : IN718 nickel-based superalloy held for 1 hour at 850°C
System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al
Reflected light microscopy, cross-polarised, with Nomarski filter
25 μm
Link to full record for micrograph 716 Micrograph 716 : IN718 nickel-based superalloy held for 3 hours at 850°C
System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al
Reflected light microscopy, cross-polarised, with Nomarski filter
25 μm

Showing 461 - 470 of 535 micrographs Page 1 .. 44 45 46 47 48 49 50 .. 54 | Previous | Next