Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Keyword
535 micrographs for keyword alloy, ordered by micrograph number.
| Showing 471 - 480 of 535 micrographs | Page 1 .. 45 46 47 48 49 50 51 .. 54 | Previous | Next |
![]() |
Micrograph
717
:
IN718 nickel-based superalloy held for 6 hours at 850°C System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al Reflected light microscopy, cross-polarised, with Nomarski filter 25 μm |
![]() |
Micrograph
718
:
IN718 nickel-based superalloy held for 24 hours at 850°C System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al Reflected light microscopy, cross-polarised, with Nomarski filter 25 μm |
![]() |
Micrograph
719
:
IN718 nickel-based superalloy held for 48 hours at 850°C System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al Reflected light microscopy, cross-polarised, with Nomarski filter 25 μm |
![]() |
Micrograph
720
:
IN718 nickel-based superalloy held for 72 hours at 850°C System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al Reflected light microscopy, cross-polarised, with Nomarski filter 25 μm |
![]() |
Micrograph
735
:
Dual-phase steel water quenched from 750°C System: Fe-C-X, Composition: Fe, C 0.15, Mn 1.5, Si 1.5 (wt%) Reflected light microscopy 6 μm |
![]() |
Micrograph
736
:
Dual-phase steel water quenched from 775°C System: Fe-C-X, Composition: Fe, C 0.15, Mn 1.5, Si 1.5 (wt%) Reflected light microscopy 5 μm |
![]() |
Micrograph
737
:
Dual-phase steel water quenched from 800°C System: Fe-C-X, Composition: Fe, C 0.15, Mn 1.5, Si 1.5 (wt%) Reflected light microscopy 6 μm |
![]() |
Micrograph
738
:
A medium carbon low alloyed structural steel System: Fe-C-X, Composition: Fe, C medium (wt%), with small alloy addition Reflected light microscopy 20 μm |
![]() |
Micrograph
739
:
TRIP steel annealed at 775°C for 5 mins and then hold at 400°C for 150s for austenite stabilization System: Fe-C-X, Composition: Fe, C 0.15, Mn 1.5, Si 1.5 (wt%) Reflected light microscopy 6 μm |
![]() |
Micrograph
740
:
TRIP steel annealed at 775°C for 5 mins and then hold at 400°C for 40s for austenite stabilization System: Fe-C-X, Composition: Fe, C 0.15, Mn 1.5, Si 1.5 (wt%) Reflected light microscopy 20 μm |
| Showing 471 - 480 of 535 micrographs | Page 1 .. 45 46 47 48 49 50 51 .. 54 | Previous | Next |