Micrograph
41
:
Zn, cold rolled - mechanical twins System: Zn, Composition: Not specified Reflected light microscopy 400 μm |
![]() |
Micrograph
42
:
Zn, cold rolled - mechanical twins System: Zn, Composition: Not specified Reflected light microscopy 80 μm |
![]() |
Micrograph
43
:
Fe, C 0.2 (wt%), explosively deformed - mechanical twins System: Fe-C-X, Composition: Fe, C 0.2 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
44
:
Fe, C 0.2 (wt%), explosively deformed - mechanical twins System: Fe-C-X, Composition: Fe, C 0.2 (wt%) Reflected light microscopy 80 μm |
![]() |
Micrograph
45
:
Fe, Ni 30, C 0.3 (wt%), quenched - martensite plates System: Fe-C-X, Composition: Fe, C 0.3, Ni 30 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
46
:
Fe, Ni 30, C 0.3 (wt%), quenched - martensite plates System: Fe-C-X, Composition: Fe, C 0.3, Ni 30 (wt%) Reflected light microscopy 80 μm |
![]() |
Micrograph
47
:
Al 95, Cu 5 (wt%), microsegregation - cored dendrites System: Al-Cu, Composition: Al 95, Cu 5 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
48
:
Al 95, Cu 5 (wt%), microsegregation - cored dendrites System: Al-Cu, Composition: Al 95, Cu 5 (wt%) Reflected light microscopy 80 μm |
![]() |
Micrograph
49
:
Cu 60, Zn 40 (wt%), slow cooling - equiaxed grains System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
50
:
Cu 60, Zn 40 (wt%), slow cooling - equiaxed grains System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) Reflected light microscopy 80 μm |
| Showing 41 - 50 of 535 micrographs | Page 1 2 3 4 5 6 7 8 .. 54 | Previous | Next |