Keyword
6 micrographs for keyword metastable, ordered by micrograph number.
![]() |
Micrograph
27
:
Fe, C 0.9 (wt%), martensite System: Fe-C-X, Composition: Fe, C 0.9 (wt%) Reflected light microscopy 40 μm |
![]() |
Micrograph
36
:
Cu 60, Zn 40 (wt%), quenched - metastable b grains System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
45
:
Fe, Ni 30, C 0.3 (wt%), quenched - martensite plates System: Fe-C-X, Composition: Fe, C 0.3, Ni 30 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
46
:
Fe, Ni 30, C 0.3 (wt%), quenched - martensite plates System: Fe-C-X, Composition: Fe, C 0.3, Ni 30 (wt%) Reflected light microscopy 80 μm |
![]() |
Micrograph
56
:
Al 96, Cu 4 (wt%), solution treated and overaged - precipitation hardening System: Al-Cu, Composition: Al 96, Cu 4 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
57
:
Al 96, Cu 4 (wt%), solution treated and overaged - precipitation hardening System: Al-Cu, Composition: Al 96, Cu 4 (wt%) Reflected light microscopy 80 μm |