1 micrograph for keyword polyhedral, ordered by micrograph number.
![]() |
Micrograph
601
:
Spherulites in in poly-3-hydroxy butyrate (PHB) System: Polyhydroxybutyrate (PHB), Composition: Not specified Cross-polarised light microscopy 240 nm |