Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Keyword
3 micrographs for keyword salt, ordered by micrograph number.
![]() |
Micrograph
628
:
Sintered salt (NaCl) System: Na-Cl, Composition: Not specified Scanning electron microscopy (SEM) 140 μm |
![]() |
Micrograph
631
:
Coarse open celled aluminium foam produced by infiltration of sintered salt (FOAM-U-LIKE) System: Al, Composition: Not specified Photography (no microscope) 6 mm |
![]() |
Micrograph
635
:
Open celled aluminium foam produced by infiltration of sintered salt System: Al, Composition: Not specified Scanning electron microscopy (SEM) 400 μm |