Keyword
2 micrographs for keyword stress, ordered by micrograph number.
![]() |
Micrograph
570
:
Strain-induced birefringence in a notched polycarbonate bar System: Polycarbonate (PC), Composition: Not specified Cross-polarised light microscopy 6 mm |
![]() |
Micrograph
571
:
Strain-induced birefringence in a polycarbonate bar System: Polycarbonate (PC), Composition: Not specified Cross-polarised light microscopy 14 mm |