57 micrographs for keyword pearlite, ordered by micrograph number.
Showing 31 - 40 of 57 micrographs | Page 1 2 3 4 5 6 | Previous | Next |
![]() |
Micrograph
234
:
Hypoeutectoid steel, normalised at 1100°C System: Fe-C-X, Composition: Fe, C 0.4 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
235
:
Hypoeutectoid steel, normalised at 950°C System: Fe-C-X, Composition: Fe, C 0.4 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
236
:
Hypoeutectoid steel, normalised at 950°C System: Fe-C-X, Composition: Fe, C 0.4 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
237
:
Hypoeutectoid steel, normalised at 950°C System: Fe-C-X, Composition: Fe, C 0.4 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
238
:
Hypoeutectoid steel, normalised at 950°C System: Fe-C-X, Composition: Fe, C 0.4 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
239
:
Fe, C 0.4, Mn 0.8 (wt%) steel, normalised System: Fe-C-X, Composition: Fe, C 0.4, Mn 0.8 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
240
:
Fe, C 0.4, Mn 0.8 (wt%) steel, normalised System: Fe-C-X, Composition: Fe, C 0.4, Mn 0.8 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
241
:
Fe, C 0.3 (wt%) steel, spheroidised carbide System: Fe-C-X, Composition: Fe, C 0.3 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
242
:
Fe, C 0.3 (wt%) steel, spheroidised carbide System: Fe-C-X, Composition: Fe, C 0.3 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
777
:
Grey cast iron (flake graphite) System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5 (wt%) Reflected light microscopy 100 μm |