Keyword
57 micrographs for keyword pearlite, ordered by micrograph number.
| Showing 41 - 50 of 57 micrographs | Page 1 2 3 4 5 6 | Previous | Next |
![]() |
Micrograph
778
:
Grey cast iron (flake graphite) System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5 (wt%) Reflected light microscopy 40 μm |
![]() |
Micrograph
779
:
Spheroidal graphite cast iron System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5, Mg 0.05 (wt%) Reflected light microscopy 50 μm |
![]() |
Micrograph
780
:
Heat treated spheroidal graphite cast iron System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5, Mg 0.05 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
781
:
Heat treated spheroidal graphite cast iron System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5, Mg 0.05 (wt%) Reflected light microscopy 50 μm |
![]() |
Micrograph
782
:
Austempered ductile cast iron System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
783
:
Austempered ductile cast iron System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
784
:
Austempered ductile cast iron System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
785
:
Austempered ductile cast iron System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%) Reflected light microscopy 20 μm |
![]() |
Micrograph
786
:
Austempered ductile cast iron System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
787
:
Austempered ductile cast iron System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%) Reflected light microscopy 20 μm |