Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Keyword
14 micrographs for keyword hypoeutectic, ordered by micrograph number.
| Showing 1 - 10 of 14 micrographs | Page 1 2 | Previous | Next |
![]() |
Micrograph
1
:
Al 75, Cu 25 (wt%), hypoeutectic alloy System: Al-Cu, Composition: Al 75, Cu 25 (wt%) Reflected light microscopy 40 μm |
![]() |
Micrograph
2
:
Al 75, Cu 25 (wt%), hypoeutectic alloy System: Al-Cu, Composition: Al 75, Cu 25 (wt%) Scanning electron microscopy (SEM) 30 μm |
![]() |
Micrograph
66
:
Hypoeutectic white cast iron System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 400 μm |
![]() |
Micrograph
67
:
Hypoeutectic white cast iron System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 80 μm |
![]() |
Micrograph
695
:
Cu-4.5 wt% P System: Cu-P, Composition: Cu 95.5, P 4.5 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
696
:
Cu-4.5 wt% P System: Cu-P, Composition: Cu 95.5, P 4.5 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
697
:
Cu-4.5 wt% P System: Cu-P, Composition: Cu 95.5, P 4.5 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
698
:
Cu-4.5 wt% P System: Cu-P, Composition: Cu 95.5, P 4.5 (wt%) Reflected light microscopy 50 μm |
![]() |
Micrograph
699
:
Cu-4.5 wt% P System: Cu-P, Composition: Cu 95.5, P 4.5 (wt%) Reflected light microscopy 20 μm |
![]() |
Micrograph
700
:
Cu-10.5 wt% P System: Cu-P, Composition: Cu 89.5, P 10.5 (wt%) Reflected light microscopy 400 μm |
| Showing 1 - 10 of 14 micrographs | Page 1 2 | Previous | Next |