Keyword
4 micrographs for keyword decarburisation, ordered by micrograph number.
![]() |
Micrograph
268
:
Fe, C 0.5 (wt%) steel, near a decarburised surface System: Fe-C-X, Composition: Fe, C 0.5 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
779
:
Spheroidal graphite cast iron System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5, Mg 0.05 (wt%) Reflected light microscopy 50 μm |
![]() |
Micrograph
780
:
Heat treated spheroidal graphite cast iron System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5, Mg 0.05 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
781
:
Heat treated spheroidal graphite cast iron System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5, Mg 0.05 (wt%) Reflected light microscopy 50 μm |