Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Keyword
1 micrograph for keyword deformation, ordered by micrograph number.
![]() |
Micrograph
710
:
Wrought-grade aluminium alloy (Al-Mg-Fe-Si containing < 1wt.% of each solute); refined with TiB2 particles. Deformation of grain structure is due to cutting of sample with scissors. System: Al-Mg-Fe-Si, Composition: Not specified Cross-polarised light microscopy 400 μm |