Dissemination of IT for the Promotion of Materials Science (DoITPoMS)

Keyword

535 micrographs for keyword metal, ordered by micrograph number.


Showing 131 - 140 of 535 micrographs Page 1 .. 11 12 13 14 15 16 17 .. 54 | Previous | Next

Link to full record for micrograph 232 Micrograph 232 : Normalised steel
System: Fe-C-X, Composition: Fe, C 0.6 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 233 Micrograph 233 : Hypoeutectoid steel, normalised at 1100°C
System: Fe-C-X, Composition: Fe, C 0.4 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 234 Micrograph 234 : Hypoeutectoid steel, normalised at 1100°C
System: Fe-C-X, Composition: Fe, C 0.4 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 235 Micrograph 235 : Hypoeutectoid steel, normalised at 950°C
System: Fe-C-X, Composition: Fe, C 0.4 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 236 Micrograph 236 : Hypoeutectoid steel, normalised at 950°C
System: Fe-C-X, Composition: Fe, C 0.4 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 237 Micrograph 237 : Hypoeutectoid steel, normalised at 950°C
System: Fe-C-X, Composition: Fe, C 0.4 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 238 Micrograph 238 : Hypoeutectoid steel, normalised at 950°C
System: Fe-C-X, Composition: Fe, C 0.4 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 239 Micrograph 239 : Fe, C 0.4, Mn 0.8 (wt%) steel, normalised
System: Fe-C-X, Composition: Fe, C 0.4, Mn 0.8 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 240 Micrograph 240 : Fe, C 0.4, Mn 0.8 (wt%) steel, normalised
System: Fe-C-X, Composition: Fe, C 0.4, Mn 0.8 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 241 Micrograph 241 : Fe, C 0.3 (wt%) steel, spheroidised carbide
System: Fe-C-X, Composition: Fe, C 0.3 (wt%)
Reflected light microscopy
400 μm

Showing 131 - 140 of 535 micrographs Page 1 .. 11 12 13 14 15 16 17 .. 54 | Previous | Next

List all keywords