535 micrographs for keyword metal, ordered by micrograph number.


Showing 211 - 220 of 535 micrographs Page 1 .. 19 20 21 22 23 24 25 .. 54 | Previous | Next

Link to full record for micrograph 315 Micrograph 315 : Fe, C 0.9 (wt%) steel, hypereutectoid, quenched and tempered
System: Fe-C-X, Composition: Fe, C 0.9 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 316 Micrograph 316 : Fe, C 0.9 (wt%) steel, hypereutectoid, quenched
System: Fe-C-X, Composition: Fe, C 0.9 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 317 Micrograph 317 : Fe, C 0.9 (wt%) steel, hypereutectoid, quenched
System: Fe-C-X, Composition: Fe, C 0.9 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 318 Micrograph 318 : Fe, C 0.9 (wt%) steel, hypereutectoid, quenched
System: Fe-C-X, Composition: Fe, C 0.9 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 326 Micrograph 326 : Low alloy medium carbon steel, isothermally transformed
System: Fe-C-X, Composition: Fe, C 0.4, Ni 1.3, Cr 0.65, Mo 0.65 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 327 Micrograph 327 : Low alloy medium carbon steel, isothermally transformed
System: Fe-C-X, Composition: Fe, C 0.4, Ni 1.3, Cr 0.65, Mo 0.65 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 328 Micrograph 328 : Nickel low carbon steel, quenched and tempered
System: Fe-C-X, Composition: Fe, C 0.31, Ni 3.0, Cr 0.9, Mn 0.6 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 329 Micrograph 329 : Nickel low carbon steel, quenched and tempered
System: Fe-C-X, Composition: Fe, C 0.31, Ni 3.0, Cr 0.9, Mn 0.6 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 330 Micrograph 330 : Near eutectoid steel, quenched to produce martensite
System: Fe-C-X, Composition: Fe, C 0.86 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 331 Micrograph 331 : Near eutectoid steel, quenched to produce martensite
System: Fe-C-X, Composition: Fe, C 0.86 (wt%)
Reflected light microscopy
100 μm

Showing 211 - 220 of 535 micrographs Page 1 .. 19 20 21 22 23 24 25 .. 54 | Previous | Next