Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Keyword
535 micrographs for keyword metal, ordered by micrograph number.
| Showing 451 - 460 of 535 micrographs | Page 1 .. 43 44 45 46 47 48 49 .. 54 | Previous | Next |
![]() |
Micrograph
697
:
Cu-4.5 wt% P System: Cu-P, Composition: Cu 95.5, P 4.5 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
698
:
Cu-4.5 wt% P System: Cu-P, Composition: Cu 95.5, P 4.5 (wt%) Reflected light microscopy 50 μm |
![]() |
Micrograph
699
:
Cu-4.5 wt% P System: Cu-P, Composition: Cu 95.5, P 4.5 (wt%) Reflected light microscopy 20 μm |
![]() |
Micrograph
700
:
Cu-10.5 wt% P System: Cu-P, Composition: Cu 89.5, P 10.5 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
701
:
Cu-10.5 wt% P System: Cu-P, Composition: Cu 89.5, P 10.5 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
702
:
Cu-10.5 wt% P System: Cu-P, Composition: Cu 89.5, P 10.5 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
703
:
Cu-10.5 wt% P System: Cu-P, Composition: Cu 89.5, P 10.5 (wt%) Reflected light microscopy 50 μm |
![]() |
Micrograph
704
:
Cu-10.5 wt% P System: Cu-P, Composition: Cu 89.5, P 10.5 (wt%) Reflected light microscopy 20 μm |
![]() |
Micrograph
705
:
Cu-? wt% P System: Cu-P, Composition: Not specified Reflected light microscopy 400 μm |
![]() |
Micrograph
706
:
Cu-? wt% P System: Cu-P, Composition: Not specified Reflected light microscopy 200 μm |
| Showing 451 - 460 of 535 micrographs | Page 1 .. 43 44 45 46 47 48 49 .. 54 | Previous | Next |