Keyword
2 micrographs for keyword TRIP steel, ordered by micrograph number.
![]() |
Micrograph
739
:
TRIP steel annealed at 775°C for 5 mins and then hold at 400°C for 150s for austenite stabilization System: Fe-C-X, Composition: Fe, C 0.15, Mn 1.5, Si 1.5 (wt%) Reflected light microscopy 6 μm |
![]() |
Micrograph
740
:
TRIP steel annealed at 775°C for 5 mins and then hold at 400°C for 40s for austenite stabilization System: Fe-C-X, Composition: Fe, C 0.15, Mn 1.5, Si 1.5 (wt%) Reflected light microscopy 20 μm |