Keyword
5 micrographs for keyword silal, ordered by micrograph number.
![]() |
Micrograph
70
:
Silal System: Fe-C-X, Composition: Fe, C 3.0, Si 6, Mn 0.7, P 0.3, S 0.1 (wt% typical) (Silal) Reflected light microscopy 200 μm |
![]() |
Micrograph
71
:
Silal System: Fe-C-X, Composition: Fe, C 3.0, Si 6, Mn 0.7, P 0.3, S 0.1 (wt% typical) (Silal) Reflected light microscopy 80 μm |
![]() |
Micrograph
387
:
Silal System: Fe-C-X, Composition: Fe, C 2.10, Si 5.60, Mn 0.50 (wt%) (Silal) Reflected light microscopy 400 μm |
![]() |
Micrograph
388
:
Silal System: Fe-C-X, Composition: Fe, C 2.10, Si 5.60, Mn 0.50 (wt%) (Silal) Reflected light microscopy 200 μm |
![]() |
Micrograph
389
:
Silal System: Fe-C-X, Composition: Fe, C 2.10, Si 5.60, Mn 0.50 (wt%) (Silal) Reflected light microscopy 100 μm |