Micrograph
372
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 3.62, Si 0.33, Mn 0.38, Cr 0.89 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
373
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 3.62, Si 0.33, Mn 0.38, Cr 0.89 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
376
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 3.56, Si 0.20, Mn 0.37, Cr 0.91 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
377
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 3.56, Si 0.20, Mn 0.37, Cr 0.91 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
384
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 2.3, Mn 4.0 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
385
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 2.3, Mn 4.0 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
386
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 2.3, Mn 4.0 (wt%) Reflected light microscopy 200 μm |