185 micrographs for keyword copper, ordered by micrograph number.
| Showing 121 - 130 of 185 micrographs | Page 1 .. 10 11 12 13 14 15 16 .. 19 | Previous | Next |
![]() |
Micrograph
514
:
Leaded gun metal bronze. System: Cu-Sn, Composition: Cu 85, Sn 5, Zn 5, Pb 5 (wt% approx) Reflected light microscopy 100 μm |
![]() |
Micrograph
515
:
Leaded gun metal bronze. System: Cu-Sn, Composition: Cu 85, Sn 5, Zn 5, Pb 5 (wt% approx) Reflected light microscopy 400 μm |
![]() |
Micrograph
516
:
Gun metal bronze displaying coring. System: Cu-Sn, Composition: Cu 88, Sn 8, Zn 4 (wt% approx) Reflected light microscopy 800 μm |
![]() |
Micrograph
517
:
Gun metal bronze displaying coring. System: Cu-Sn, Composition: Cu 88, Sn 8, Zn 4 (wt% approx) Reflected light microscopy 400 μm |
![]() |
Micrograph
518
:
Gun metal bronze displaying coring. System: Cu-Sn, Composition: Cu 88, Sn 8, Zn 4 (wt% approx) Reflected light microscopy 200 μm |
![]() |
Micrograph
519
:
Gun metal bronze displaying coring. System: Cu-Sn, Composition: Cu 88, Sn 8, Zn 4 (wt% approx) Reflected light microscopy 100 μm |
![]() |
Micrograph
520
:
Cu - 5% Sn phosphor bronze. System: Cu-Sn, Composition: Cu 95, Sn 5, P 0.15 (wt% approx) Reflected light microscopy 400 μm |
![]() |
Micrograph
521
:
Cu - 5% Sn phosphor bronze. System: Cu-Sn, Composition: Cu 95, Sn 5, P 0.15 (wt% approx) Reflected light microscopy 200 μm |
![]() |
Micrograph
522
:
Cu - 5% Sn phosphor bronze. System: Cu-Sn, Composition: Cu 95, Sn 5, P 0.15 (wt% approx) Reflected light microscopy 100 μm |
![]() |
Micrograph
523
:
Phosphor bronze exhibiting cored dendrites. System: Cu-Sn, Composition: Cu 90, Sn 10 (wt%) + P trace Reflected light microscopy 400 μm |
| Showing 121 - 130 of 185 micrographs | Page 1 .. 10 11 12 13 14 15 16 .. 19 | Previous | Next |