185 micrographs for keyword copper, ordered by micrograph number.
| Showing 51 - 60 of 185 micrographs | Page 1 .. 3 4 5 6 7 8 9 .. 19 | Previous | Next |
![]() |
Micrograph
437
:
Cu, Sn 20 (wt%) bronze, exhibiting dendritic solidification System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
438
:
Cu, Sn 20 (wt%) bronze, exhibiting dendritic solidification System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
439
:
a b nickel brass containing 2% lead. System: Cu-Zn, Composition: Cu 46, Zn 42, Ni 10, Pb 2 (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
440
:
a b nickel brass containing 2% lead. System: Cu-Zn, Composition: Cu 46, Zn 42, Ni 10, Pb 2 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
441
:
Cu 60, Zn 40 (wt%) brass, Widmanstätten microstructure System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
442
:
Cu 60, Zn 40 (wt%) brass, Widmanstätten microstructure System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
443
:
Commercial grade free machining brass - Widmanstätten microstructure System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) + Pb trace Reflected light microscopy 400 μm |
![]() |
Micrograph
444
:
Commercial grade free machining brass - Widmanstätten microstructure System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) + Pb trace Reflected light microscopy 200 μm |
![]() |
Micrograph
445
:
Cast and annealed 40 wt% Zn brass System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) + Pb trace Reflected light microscopy 400 μm |
![]() |
Micrograph
446
:
Cast and annealed 40 wt% Zn brass System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) + Pb trace Reflected light microscopy 200 μm |