185 micrographs for keyword copper, ordered by micrograph number.
| Showing 71 - 80 of 185 micrographs | Page 1 .. 5 6 7 8 9 10 11 .. 19 | Previous | Next |
![]() |
Micrograph
457
:
Cu 55, Zn 45 (wt%) brass, as cast, dendritic System: Cu-Zn, Composition: Cu 55, Zn 45 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
458
:
Brass, exhibiting grain boundary nucleation System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
459
:
Brass, exhibiting grain boundary nucleation System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
460
:
Brass, exhibiting grain boundary nucleation System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
468
:
Cu 50, Zn 50 (wt%) brass, as cast System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
469
:
Cu 50, Zn 50 (wt%) brass, as cast System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
470
:
Cu 50, Zn 50 (wt%) brass, as cast System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
471
:
Cu 50, Zn 50 (wt%) brass, as cast System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
472
:
Cu 50, Zn 50 (wt%) brass, chill cast System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
473
:
Cu 50, Zn 50 (wt%) brass, chill cast System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%) Reflected light microscopy 400 μm |