Keyword
272 micrographs for keyword iron, ordered by micrograph number.
Showing 171 - 180 of 272 micrographs | Page 1 .. 15 16 17 18 19 20 21 .. 28 | Previous | Next |
Micrograph
344
:
Medium carbon, low alloy steel. System: Fe-C-X, Composition: Fe, C 0.31, Ni 3.0, Cr 0.9, Mn 0.6 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
345
:
Medium carbon, low alloy steel, isothermally transformed System: Fe-C-X, Composition: Fe, C 0.4, Ni 1.3, Cr 0.65, Mo 0.65 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
346
:
Fe, C 1.35 (wt%) steel, hypereutectoid, quenched System: Fe-C-X, Composition: Fe, C 1.35 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
347
:
Fe, C 1.35 (wt%) steel, hypereutectoid, quenched System: Fe-C-X, Composition: Fe, C 1.35 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
348
:
Fe, C 1.35 (wt%) steel, hypereutectoid, quenched System: Fe-C-X, Composition: Fe, C 1.35 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
349
:
Fe, C 1.35 (wt%) steel, hypereutectoid, quenched System: Fe-C-X, Composition: Fe, C 1.35 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
350
:
Fe, C 0.15 (wt%) steel, quenched. System: Fe-C-X, Composition: Fe, C 0.15 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
351
:
Fe, C 0.15 (wt%) steel, quenched. System: Fe-C-X, Composition: Fe, C 0.15 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
352
:
Fe, C 0.15 (wt%) steel, quenched. System: Fe-C-X, Composition: Fe, C 0.15 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
353
:
Pearlitic malleable cast iron System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 800 μm |
Showing 171 - 180 of 272 micrographs | Page 1 .. 15 16 17 18 19 20 21 .. 28 | Previous | Next |