Keyword
272 micrographs for keyword iron, ordered by micrograph number.
Showing 181 - 190 of 272 micrographs | Page 1 .. 16 17 18 19 20 21 22 .. 28 | Previous | Next |
Micrograph
354
:
Pearlitic malleable cast iron System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 400 μm |
|
Micrograph
355
:
Pearlitic malleable cast iron System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 200 μm |
|
Micrograph
356
:
Pearlitic malleable cast iron System: Fe-C-X, Composition: Fe, C 2.4, Si 1.1, Mn 1.1 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
357
:
Pearlitic malleable cast iron System: Fe-C-X, Composition: Fe, C 2.4, Si 1.1, Mn 1.1 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
358
:
White cast iron, annealed to precipitate out carbon System: Fe-C-X, Composition: Fe, C 2.4, Si 1.1, Mn 1.1 (wt%) Reflected light microscopy 800 μm |
|
Micrograph
359
:
White cast iron, annealed to precipitate out carbon System: Fe-C-X, Composition: Fe, C 2.4, Si 1.1, Mn 1.1 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
360
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 2.4, Si 1.1, Mn 1.1 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
361
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 2.4, Si 1.1, Mn 1.1 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
362
:
White cast iron, subject to slow heating and cooling treatment System: Fe-C-X, Composition: Fe, C 3.4, Si 0.35, Mn 0.22 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
363
:
White cast iron, subject to slow heating and cooling treatment System: Fe-C-X, Composition: Fe, C 3.4, Si 0.35, Mn 0.22 (wt%) Reflected light microscopy 400 μm |